Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Terblend® N NM-19 XP - (ABS+PA6) - INEOS Styrolution

Material Data Center offers the following functions for Terblend® N NM-19 XP:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Terblend N datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Terblend® N NM-19 XP is an UV stabilised ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearance.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 40 / * cm³/10min ISO 1133
Température 240 / * °C -
Charge 10 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 / * % ISO 294-4, 2577
Densité du fondu 928 kg/m³ -
Conductivité thermique du fondu 0.156 W/(m K) -
Chaleur spécifique du fondu 2410 J/(kg K) -
Température d'éjection 90 °C -
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 2000 / 1400 MPa ISO 527
Contrainte d'écoulement 43 / 34 MPa ISO 527
Déformation au seuil d'écoulement 3.5 / 5.5 % ISO 527
Déformation nominale à la rupture 30 / 35 % ISO 527
Résistance au choc Charpy, +23°C N / - kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 65 / - kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 15 / - kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 65 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 85 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 102 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 100 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 3.2 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.3 / - - IEC 62631-2-1
Permittivité relative, 1MHz 2.9 / 3.3 - IEC 62631-2-1
Facteur de pertes, 1MHz 150 / 550 E-4 IEC 62631-2-1
Résistivité transversale >1E13 / 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E14 Ohm IEC 62631-3-2
Indice de résistance au cheminement 600 / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'humidité 1.2 / * % Sim. to ISO 62
Masse volumique 1070 / - kg/m³ ISO 1183
Fonctions
Module de cisaillement dynamique / Température , Terblend® N NM-19 XP, (ABS+PA6), INEOS Styrolution
Contrainte / Déformation (isochrone) 23°C, Terblend® N NM-19 XP (cond.), (ABS+PA6), INEOS Styrolution
Module de fluage / Temps 23°C, Terblend® N NM-19 XP (cond.), (ABS+PA6), INEOS Styrolution
Courbe de fluage 23°C, Terblend® N NM-19 XP (cond.), (ABS+PA6), INEOS Styrolution
Contrainte / Déformation (isochrone) 60°C, Terblend® N NM-19 XP (sec), (ABS+PA6), INEOS Styrolution
Module de fluage / Temps 60°C, Terblend® N NM-19 XP (sec), (ABS+PA6), INEOS Styrolution
Courbe de fluage 60°C, Terblend® N NM-19 XP (sec), (ABS+PA6), INEOS Styrolution
Volume spécifique (pvT) , Terblend® N NM-19 XP, (ABS+PA6), INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 240 - 270 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
Résistance Chimique
Acides
Acide nitrique (masse en 40%) (23°C)
Acide sulfurique (masse en 38%) (23°C)
Acide chromique (masse en 40%) (23°C)
Cetones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Autres
Acétate d'éthyle (23°C)
Peroxyde d'hydrogene (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.